Boli ste presmerovaní na lokálnu verziu požadovanej stránky

Copper in nickel plating bath

AN-V-150

en

The concentration of Cu in a Ni plating bath is determined by polarography in chloride-containing acetate buffer at pH 4.7.

The concentration of Cu in a Ni plating bath is determined by polarography in chloride-containing acetate buffer at pH 4.7.