Iron in deoxidation solution (oxalate method)

AN-V-162

en

The concentration of Fe(total) is determined by polarography in oxalate buffer pH 2. This method is suitable for iron concentrations in the mg/L range.

The concentration of Fe(total) is determined by polarography in oxalate buffer pH 2. This method is suitable for iron concentrations in the mg/L range.